Please use this identifier to cite or link to this item: https://repositorio.ufrn.br/handle/123456789/31602
Full metadata record
DC FieldValueLanguage
dc.contributor.authorMartinelli, Antonio Eduardo-
dc.contributor.authorSampaio, Z. L. M.-
dc.contributor.authorGomes, T. S.-
dc.date.accessioned2021-02-22T18:41:40Z-
dc.date.available2021-02-22T18:41:40Z-
dc.date.issued2017-12-
dc.identifier.citationSAMPAIO, Z. L. M.; MARTINELLI, A. E.; GOMES, T. S.. Formulation and characterization of structural lightweight concrete containing residues of porcelain tile polishing, tire rubber and limestone. Cerâmica, [S.L.], v. 63, n. 368, p. 530-535, dez. 2017. FapUNIFESP (SciELO). http://dx.doi.org/10.1590/0366-69132017633682139. Disponível em: http://www.scielo.br/scielo.php?script=sci_arttext&pid=S0366-69132017000400530&lng=en&tlng=en. Acesso em: 13 jan. 2021.pt_BR
dc.identifier.issn1678-4553-
dc.identifier.urihttps://repositorio.ufrn.br/handle/123456789/31602-
dc.description.abstractO recente aumento da indústria da construção civil transformou o concreto em uma escolha ideal para reciclar vários resíduos que anteriormente eram descartados no meio ambiente. Entre os vários produtos, os resíduos de polimento de porcelanato, calcário e borracha de pneus são candidatos potenciais para substituir agregados miúdos nas misturas convencionais. O objetivo deste estudo foi investigar o efeito da adição de diferentes teores desses resíduos no concreto leve, onde a argila expandida substituiu a brita. Para tal, foram realizados ensaios de abatimento, resistência à compressão, densidade, índice de vazios, porosidade e absorção. As densidades de todas as formulações de concreto estudadas foram 10% inferiores às do concreto leve (<1,850 kg/m³). No entanto, misturas contendo 10 a 15% de resíduos combinados representaram redução da absorção, índice de vazios e porosidade em pelo menos 17% em comparação com o concreto convencional. A resistência de tais formulações atingiu 27 MPa aos 28 dias com consistência de 9 a 12 cm, indicando consistência adequada e aumento na resistência à compressão. Além disso, a combinação de baixa porosidade, absorção e vazios sugeriu maior durabilidade ao concretopt_BR
dc.languageenpt_BR
dc.publisherABCERAMpt_BR
dc.rightsAttribution-NonCommercial 3.0 Brazil*
dc.rights.urihttp://creativecommons.org/licenses/by-nc/3.0/br/*
dc.subjectLightweight concretept_BR
dc.subjectPorcelain tile polishing residuept_BR
dc.subjectTire rubber residuept_BR
dc.subjectLimestone residuept_BR
dc.titleFormulation and characterization of structural lightweight concrete containing residues of porcelain tile polishing, tire rubber and limestonept_BR
dc.title.alternativeFormulação e caracterização de concreto leve estrutural contendo resíduos de polimento de porcelanato, borracha de pneus e calcáriopt_BR
dc.typearticlept_BR
dc.identifier.doi10.1590/0366-69132017633682139-
dc.description.resumoThe recent increase in the construction industry has transformed concrete into an ideal choice to recycle a number of residues formerly discarded into the environment. Among various products, porcelain tile polishing, limestone and tire rubber residues are potential candidates to replace the fine aggregate of conventional mixtures. The aim of this study was to investigate the effect of the addition of varying contents of these residues in lightweight concrete where expanded clay replaced gravel. To that end, slump, compressive strength, density, void ratio, porosity and absorption tests were carried out. The densities of all concrete formulations studied were 10% lower to that of lightweight concrete (<1.850 kg/m³). Nevertheless, mixes containing 10 to 15% of combined residues reduced absorption, void ratio and porosity, at least 17% lower compared to conventional concrete. The strength of such formulations reached 27 MPa at 28 days with consistency of 9 to 12 cm, indicating adequate consistency and increased strength. In addition, the combination of low porosity, absorption and voids suggested improved durabilitypt_BR
Appears in Collections:CT - DEMAT - Artigos publicados em periódicos

Files in This Item:
File Description SizeFormat 
FormulationCharacterization_MARTINELLI_2017.pdf561.2 kBAdobe PDFThumbnail
View/Open


This item is licensed under a Creative Commons License Creative Commons