Shear bond strength of veneering porcelain to zirconia: Effect of surface treatment by CNC-milling and composite layer deposition on zirconia

dc.contributor.authorNascimento, Rubens Maribondo do
dc.contributor.authorSantos, Rafaela Luiz Pereira
dc.contributor.authorSilva, Filipe Samuel
dc.contributor.authorSouza, Júlio César Matias de
dc.contributor.authorMotta, Fabiana Villela da
dc.contributor.authorCarvalho, Oscar
dc.contributor.authorHenriques, Bruno
dc.date.accessioned2022-01-05T14:24:36Z
dc.date.available2022-01-05T14:24:36Z
dc.date.issued2016-07
dc.description.resumoObjectives: The purpose of this study was to evaluate the shear bond strength of veneering feldspathic porcelain to zirconia substrates modified by CNC-milling process or by coating zirconia with a composite interlayer. Methods: Four types of zirconia–porcelain interface configurations were tested: RZ – porcelain bonded to rough zirconia substrate (n1⁄416); PZ – porcelain bonded to zirconia substrate with surface holes (n1⁄416); RZI – application of a composite interlayer between the veneering porcelain and the rough zirconia substrate (n1⁄416); PZI – application of a composite interlayer between the porcelain and the zirconia substrate treated by CNC-milling (n1⁄416). The composite interlayer was composed of zirconia particles reinforced porcelain (30%, vol%). The mechanical properties of the ceramic composite have been determined. The shear bond strength test was performed at 0.5 mm/min using a universal testing machine. The interfaces of fractured and untested specimens were examined by FEG-SEM/EDS. Data was analyzed with Shapiro–Wilk test to test the assumption of normality. The one-way ANOVA followed by Tukey HSD multiple comparison test was used to compare shear bond strength results (α1⁄40.05). Results: The shear bond strength of PZ (100715 MPa) and RZI (96711 MPa) specimens were higher than that recorded for RZ (control group) specimens (89715 MPa), although not significantly (p40.05). The highest shear bond strength values were recorded for PZI specimens (138719 MPa), yielding a significant improvement of 55% relative to RZ specimens (po0.05)pt_BR
dc.identifier.citationSANTOS, R. L. P.; SILVA, F. S.; NASCIMENTO, R. M.; SOUZA, J. C. M.; MOTTA, F. V.; CARVALHO, O.; HENRIQUES, B. Shear bond strength of veneering porcelain to zirconia: effect of surface treatment by cnc-milling and composite layer deposition on zirconia. Journal of the Mechanical Behavior of Biomedical Materials, [S.L.], v. 60, p. 547-556, jul. 2016. Disponível em: https://www.sciencedirect.com/science/article/abs/pii/S1751616116300352?via%3Dihub. Acesso em: 05 abr. 2021. http://dx.doi.org/10.1016/j.jmbbm.2016.03.015.pt_BR
dc.identifier.doi10.1016/j.jmbbm.2016.03.015
dc.identifier.issn1751-6161
dc.identifier.urihttps://repositorio.ufrn.br/handle/123456789/45569
dc.languageenpt_BR
dc.publisherElsevierpt_BR
dc.rightsAttribution-NonCommercial-NoDerivs 3.0 Brazil*
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/3.0/br/*
dc.subjectZirconiapt_BR
dc.subjectFeldspathic porcelainpt_BR
dc.subjectShear bond strengthpt_BR
dc.subjectComposite interlayerpt_BR
dc.subjectCNC-created surface holespt_BR
dc.titleShear bond strength of veneering porcelain to zirconia: Effect of surface treatment by CNC-milling and composite layer deposition on zirconiapt_BR
dc.typearticlept_BR

Arquivos

Pacote Original

Agora exibindo 1 - 1 de 1
Nenhuma Miniatura disponível
Nome:
ShearBondStrength_NASCIMENTO_2016.pdf
Tamanho:
3.84 MB
Formato:
Adobe Portable Document Format
Nenhuma Miniatura disponível
Baixar

Licença do Pacote

Agora exibindo 1 - 1 de 1
Nenhuma Miniatura disponível
Nome:
license.txt
Tamanho:
1.45 KB
Formato:
Item-specific license agreed upon to submission
Nenhuma Miniatura disponível
Baixar